Mechanical Properties Metric English Comments
Peel Strength 5.08 kN/m
29.0 pli
Bond Strength; ASTM D624
Arlon 55578R036 0.036" (0.914 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: PolyethyleneSide 2, Layer 2: Uncured Silicone Rubber Side 2, Layer 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Side 1: Cured Silicone Rubber Appearance:..
Peel Strength 5.08 kN/m
29.0 pli
on canvas
3M Scotch-Weld™ 3796 Hot Melt Adhesive
High performance for plastics and light-gauge metalsInformation provided by 3M
Peel Strength 5.08 kN/m
29.0 pli
180°, Polyacrylic
3M Scotch-Weld™ TE100 Polyurethane Reactive Adhesive
3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as ..