3M Scotch-Weld™ 3796 Hot Melt Adhesive

Category Polymer , Adhesive
Manufacturer 3M
Trade Name Scotch-Weld™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotch-Weld™ 3796 Hot Melt Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High performance for plastics and light-gauge metalsInformation provided by 3M
Physical Properties Metric English Comments
Brookfield Viscosity 23000 cP

@Temperature 191 °C
23000 cP

@Temperature 375 °F
Mechanical Properties Metric English Comments
Shear Strength 3.79 MPa
550 psi
On Douglas Fir
Peel Strength 5.08 kN/m
29.0 pli
on canvas
Thermal Properties Metric English Comments
Ring & Ball Softening Point 116 °C
241 °F
ASTM E28-99