Polymer Property : Peel Strength = 4.9375 pli Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Peel Strength 0.86554 kN/m
4.9375 pli
ABS, 90° peel, 2 mil aluminum backing, 72 hr RT; ASTM D3330
3M 9671LE Adhesive Transfer Tapes with Adhesive 300LSE
3M™ Adhesive Transfer Tapes with 3M™ Low Surface Energy Acrylic Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and p..
Peel Strength 0.86554 kN/m
4.9375 pli
Stainless Steel, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
3M 7907 Screen Printable Sheet Polyester Label Material
3M™ Screen Printable Sheet Polyester Label Material 7907 is a durable, high performance material that offers excellent thermal stability, moisture resistance and chemical resistance. This label mat..
Peel Strength 0.86554 kN/m
4.9375 pli
Polypropylene, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
3M 7907 Screen Printable Sheet Polyester Label Material
3M™ Screen Printable Sheet Polyester Label Material 7907 is a durable, high performance material that offers excellent thermal stability, moisture resistance and chemical resistance. This label mat..
Peel Strength 0.86554 kN/m
4.9375 pli
90° Peel, PET/Aluminum, 72 hrs at 70°C0; ASTM D3330
3M 7993MP Hi-Performance Acrylic 200MP
This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia..
Peel Strength 0.86554 kN/m
4.9375 pli
ABS, 90° peel, 2 mil aluminum backing, 72 hr RT; ASTM D3330
3M 8132LE Adhesive Transfer Tapes with Adhesive 300LSE
3M™ Adhesive Transfer Tapes with 3M™ Low Surface Energy Acrylic Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and p..
Peel Strength 0.86554 kN/m
4.9375 pli
ABS, 90° peel, 2 mil aluminum backing, 72 hr RT; ASTM D3330
3M 9471FL Adhesive Transfer Tape with 300LSE Adhesive
Features:Clear Polyester (PET)Quick flowing acrylic adhesive speeds lamination processExcellent initial adhesion, especially to LSE (low surface energy) plasticsBonds graphics to powder coatings, LS..
Peel Strength 0.86554 kN/m
4.9375 pli
ABS, 90° peel, 2 mil aluminum backing, 72 hr RT; ASTM D3330
3M 9471LE Adhesive Transfer Tapes with Adhesive 300LSE
3M™ Adhesive Transfer Tapes with 3M™ Low Surface Energy Acrylic Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and p..