Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 0.86554 kN/m | 4.9375 pli | ABS, 90° peel, 2 mil aluminum backing, 72 hr RT; ASTM D3330 |
3M 9671LE Adhesive Transfer Tapes with Adhesive 300LSE 3M™ Adhesive Transfer Tapes with 3M™ Low Surface Energy Acrylic Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and p.. |
|||
Peel Strength | 0.86554 kN/m | 4.9375 pli | Stainless Steel, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7907 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Material 7907 is a durable, high performance material that offers excellent thermal stability, moisture resistance and chemical resistance. This label mat.. |
|||
Peel Strength | 0.86554 kN/m | 4.9375 pli | Polypropylene, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7907 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Material 7907 is a durable, high performance material that offers excellent thermal stability, moisture resistance and chemical resistance. This label mat.. |
|||
Peel Strength | 0.86554 kN/m | 4.9375 pli | 90° Peel, PET/Aluminum, 72 hrs at 70°C0; ASTM D3330 |
3M 7993MP Hi-Performance Acrylic 200MP This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia.. |
|||
Peel Strength | 0.86554 kN/m | 4.9375 pli | ABS, 90° peel, 2 mil aluminum backing, 72 hr RT; ASTM D3330 |
3M 8132LE Adhesive Transfer Tapes with Adhesive 300LSE 3M™ Adhesive Transfer Tapes with 3M™ Low Surface Energy Acrylic Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and p.. |
|||
Peel Strength | 0.86554 kN/m | 4.9375 pli | ABS, 90° peel, 2 mil aluminum backing, 72 hr RT; ASTM D3330 |
3M 9471FL Adhesive Transfer Tape with 300LSE Adhesive Features:Clear Polyester (PET)Quick flowing acrylic adhesive speeds lamination processExcellent initial adhesion, especially to LSE (low surface energy) plasticsBonds graphics to powder coatings, LS.. |
|||
Peel Strength | 0.86554 kN/m | 4.9375 pli | ABS, 90° peel, 2 mil aluminum backing, 72 hr RT; ASTM D3330 |
3M 9471LE Adhesive Transfer Tapes with Adhesive 300LSE 3M™ Adhesive Transfer Tapes with 3M™ Low Surface Energy Acrylic Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and p.. |