Peel Strength 3.77 kN/m
21.5 pli
Bond Strength; ASTM D624
Arlon 51581R028 0.028" (0.711 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone Rubber Interleave 2: Polyethylene Appearance: Red silicone gu..