Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 3.77 kN/m | 21.5 pli | Bond Strength; ASTM D624 |
Arlon 51581R028 0.028" (0.711 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone Rubber Interleave 2: Polyethylene Appearance: Red silicone gu.. |