Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 4.00 - 4.80 kN/m | 22.8 - 27.4 pli | |
Permabond ES569 Epoxy Resin PERMABOND® ES569 is a single-part heat cured epoxy adhesive with excellent adhesion to metal surfaces as well as composite materials. The high bond strength of this adhesive allows it to replace me.. |
|||
Peel Strength | 3.00 - 4.80 kN/m | 17.1 - 27.4 pli | ISO 4578 |
Permabond TA4302 Toughened Acrylic Adhesive PERMABOND® TA4302 is a 2-part, 1:1 toughened acrylic adhesive. It can be used to bond a wide variety of materials including metals, plastics, GRP, ceramics, wood and other substrates. It is conveni.. |