Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 3.30 kN/m | 18.8 pli | T-Peel (CRS St 1203, 0.5mm) |
Dow BETAMATE™ XW 1185 Epoxy BETAMATE™ XW 1185 is a one component heat curing Epoxy paste adhesive. The material is readily pumped at ambient temperatures. It shows excellent adhesion to automotive steel and aluminum, is resi.. |