Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 1.93 kN/m | 11.0 pli | Copper; 1 oz. EDC After Solder Float; IPC-TM-650 2.4.8 |
Rogers Corporation RO3210 Woven-Glass Reinforced PTFE Laminate Features and Benefits:Woven glass reinforcement - Improves rigidity for easier handlingUniform electrical and mechanical performance - ideal for complex multi-layer high frequency structuresLow diel.. |
|||
Peel Strength | 1.93 kN/m | 11.0 pli | Bond Strength; Arlon SQA-TMS-011 |
Arlon 55148R036 0.036" (0.914 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 2, Layer 2: Uncured Silicone Rubber Side 2, Layer 1: Cured Silicone RubberSubstrate: Style 162 Fiberglass Side 1: Cured Silicone Rubber This data r.. |
|||
Peel Strength | 1.93 kN/m | 11.0 pli | 90°, Adhesion to Polystyrene |
3M Bumpon™ SJ5904 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Peel Strength | 1.93 kN/m | 11.0 pli | 90°, Adhesion to Polystyrene |
3M Bumpon™ SJ5908 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Peel Strength | 1.93 kN/m | 11.0 pli | 90°, Adhesion to Polystyrene |
3M Bumpon™ SJ6008 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Peel Strength | 1.93 kN/m | 11.0 pli | 90°, Adhesion to Polystyrene |
3M Bumpon™ SJ6016 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Peel Strength | 1.93 kN/m | 11.0 pli | To Copper (1 oz./35 micron); At Elevated Temperatures; IPC TM-650 2.4.8.2 |
Arlon CLTE-XT High Precision Ceramic PTFE Microwave material for improved thermal management, Excellent dimensional stability with high degree of phase stability vs. temperature.CLTE-XT is a micro-dispersed ceramic PTFE composite utilizing .. |
|||
Peel Strength | 1.93 kN/m | 11.0 pli | 90°, Adhesion to Polystyrene |
3M Bumpon™ SJ6032 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Peel Strength | 1.93 kN/m | 11.0 pli | Bond Strength; ASTM D624 |
Arlon R35928R025 0.025" (0.635 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: Polyethylene Side 1, Layer 2: Uncured Silicone RubberSide 1, Layer 1: Cured Silicone Rubber Substrate: Style 7628 Fiberglass Side 2: Cured Silicone RubberAppearance: .. |
|||
Peel Strength | 1.93 kN/m | 11.0 pli | T-Peel, Initial, Substrate failure |
3M Scotch-Weld™ TE030 Polyurethane Reactive Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as .. |
|||
Peel Strength | 1.93 kN/m | 11.0 pli | 180°, Polystyrene |
3M Scotch-Weld™ TE100 Black Polyurethane Reactive Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as .. |
|||
Peel Strength | 1.93 kN/m | 11.0 pli | 90°, Adhesion to Polystyrene |
3M SJ5300 Protective Product, Molded Shapes 3M Bumpon Protective Products Molded Shapes – Colored and Clear Series are pressure-sensitive, adhesive-back polyurethane products. They can be used as feet, stops, spaces, and protectors in many a.. |
|||
Peel Strength | 1.93 kN/m | 11.0 pli | 90°, Adhesion to Polystyrene |
3M SJ5400 Protective Product, Molded Shapes 3M Bumpon Protective Products Molded Shapes – Colored and Clear Series are pressure-sensitive, adhesive-back polyurethane products. They can be used as feet, stops, spaces, and protectors in many a.. |
|||
Peel Strength | 1.93 kN/m | 11.0 pli | [ppiw], Bond Strength to 6061 aluminum (90° peel test); Arlon SQA-TMS-011 |
Arlon 51991A020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 7628 Fiberglass Side 2: Uncured Silicone Rubber Interleave 2: Polyethylene This data represents typica.. |
|||
Peel Strength | 1.93 kN/m | 11.0 pli | 90°, Adhesion to Polystyrene |
3M Bumpon™ SJ5916 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Peel Strength | 1.93 kN/m | 11.0 pli | 180° T-Peel, Neoprene/CRS |
3M Scotch-Weld™ DP820 Acrylic Adhesives 3M™ Scotch-Weld™ Acrylic Adhesive DP820 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact and durability .. |
|||
Peel Strength | 1.93 kN/m | 11.0 pli | Polyethylene, linear, 180° after aging 1-2 days @ RT and 1 day |
3M Scotch-Weld™ Hi-Strength Postforming 4693 High Performance Industrial Plastic Adhesives Features:Low viscosity grade for spray or brush applicationClear elastomeric adhesives with high immediate bond strength, long tack range and contact bond propertiesExhibits outstanding bond strengt.. |
|||
Peel Strength | 1.93 kN/m | 11.0 pli | Polyethylene, linear, 180° after aging 1-2 days @ RT and 1 day |
3M Scotch-Weld™ Hi-Strength Postforming 4693H High Performance Industrial Plastic Adhesives Features: High Viscosity grade in collapsible tubes for flow applicationsClear elastomeric adhesives with high immediate bond strength, long tack range and contact bond propertiesExhibits outstandin.. |