Peel Strength 1.77 kN/m
10.1 pli
after solder float; IPC-TM-650.2.4.8
Park Electrochemical Nelco® N4000-29 BC® Buried Capacitance™ Multifunctional Epoxy
The Nelco N4000-29 is a lead-free, low-CTE, high Tg multifunctional epoxy substrate which has been designed for use in standard multilayer PWB designs and today’s toughest, high-performance, lead-f..
Peel Strength 1.77 kN/m
10.1 pli
Silicone Compound Property - Adhesion Strength to Aluminum; Arlon SQA-TMS-011
Arlon 90B32R016AC Aluminum Clad Press Pad with "C-Finish"
Design/Construction:Side 2: Alloy 1100 Aluminum FoilSide 1: Cured Silicone RubberThis data represents typical values for the production material and should not be used as material specifications.I..
Peel Strength 1.77 kN/m
10.1 pli
Silicone Compound Property - Adhesion Strength to Aluminum; Arlon SQA-TMS-011
Arlon 91B32R016AC Aluminum Clad Silicone Press Pad with "C-finish"
Design/Construction:Side 2: Alloy 1100 H18 Aluminum FoilSide 1: Cured Silicone RubberThis data represents typical values for the production material and should not be used as material specificatio..