Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | >= 0.240 kN/m | >= 1.37 pli | IPC-TM-650 |
CEN® Electronic Material CF 150CF019 Polyimide Film CEN®CF polyimide film is the general CEN®CN film that is coated or laminated on one or both sides with Teflon® FEP fluoropolymer. CEN®CF imparts heat sealability, provides a moisture barrier, an.. |
|||
Peel Strength | >= 0.240 kN/m | >= 1.37 pli | IPC-TM-650 |
CEN® Electronic Material CF 200CF919 Polyimide Film CEN®CF polyimide film is the general CEN®CN film that is coated or laminated on one or both sides with Teflon® FEP fluoropolymer. CEN®CF imparts heat sealability, provides a moisture barrier, an.. |
|||
Peel Strength | >= 0.240 kN/m | >= 1.37 pli | IPC-TM-650 |
CEN® Electronic Material CF 120CF616 Polyimide Film CEN®CF polyimide film is the general CEN®CN film that is coated or laminated on one or both sides with Teflon® FEP fluoropolymer. CEN®CF imparts heat sealability, provides a moisture barrier, an.. |
|||
Peel Strength | 0.240 kN/m | 1.37 pli | Average value: 0.240 kN/m Grade Count:3 |
Overview of materials for Polyimide, Thermoset Film This property data is a summary of similar materials in the MatWeb database for the category "Polyimide, Thermoset Film". Each property range of values reported is minimum and maximum values of appr.. |