Material Notes:
CEN®CF polyimide film is the general CEN®CN film that is coated or laminated on one or both sides with Teflon® FEP fluoropolymer. CEN®CF imparts heat sealability, provides a moisture barrier, and enhances chemical resistance.Applications: require a heat bondable film, or moisture and chemical resistance beyond the capabilities of uncoated CEN®CN films, such as tubing, heater circuits, heat sealable bags, automotive diaphragms and manifolds, magnetic wire, PTC InsulationAll information provided by CEN Electronic Material Co., LTD.
Physical Properties Metric English Comments
Thickness 22.0 - 28.0 microns
0.866 - 1.10 mil
Base; ASTM D374
30.0 - 36.0 microns
1.18 - 1.42 mil
Total; ASTM D374
Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 160 MPa
>= 23200 psi
ASTM D882
Elongation at Yield >= 45 %
>= 45 %
ASTM D882
Peel Strength >= 0.240 kN/m
>= 1.37 pli
IPC-TM-650
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+13 ohm-cm
>= 1.00e+13 ohm-cm
ASTM D257
Surface Resistance >= 1.00e+14 ohm
>= 1.00e+14 ohm
ASTM D257
Dielectric Strength >= 200 kV/mm
>= 5080 kV/in
ASTM D149