Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 0.105 kN/m | 0.600 pli | Adhesion to Glass |
3M Controltac™ 3552C Changeable Graphic Film with Comply™ Adhesive 2-mil white, vinyl film; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Conforms to surfaces with corrugations and rivets; Air release channels for fast, easy, bub.. |
|||
Peel Strength | 0.105 kN/m | 0.600 pli | Adhesion to Glass |
3M Controltac™ 8652C Changeable Graphic Film with Comply™ Adhesive Film 8652C is a 2-mil film with sideable, repositionable, pressure-activated adhesive. This short-term durable and removable film is an excellent choice for fleet graphics, including surfaces with c.. |
|||
Peel Strength | 0.105 kN/m | 0.600 pli | Adhesion to Fruehauf pre-painted panels |
3M Controltac™ 8655C ES Changeable Graphic Film with Comply™ Adhesive 3M™ Controlact™ Plus Changeable Graphic Film with Comply™ Adhesive 8655C ES combines the features found in Controltac and Comply adhesive technologies, including pressure activation, positionabil.. |
|||
Peel Strength | 0.105 kN/m | 0.600 pli | Adhesion to Glass |
3M Controltac™ IJ3552C Changeable Graphic Film with Comply™ Adhesive 2-mil white, vinyl film; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Conformers to surface with corrugations and rivets; Air release channels for fast, easy, bu.. |
|||
Peel Strength | 0.105 kN/m | 0.600 pli | Adhesion to Fruehauf pre-painted panels |
3M Scotchcal™ IJ355%-10 Changeable Graphic Film 4-mil, opaque white vinyl film with a matte finish; Excellent hiding power; Pressure-sensitive adhesive; Changeable for clean removable without heat or chemicalsInformation provided by 3M |
|||
Peel Strength | 0.105 kN/m | 0.600 pli | Adhesion to Fruehauf pre-painted panels |
3M Controltac™ 3500C Changeable Graphic Film with Comply™ Adhesive 4-mil, opaque white vinyl film with a matte finish; Excellent hiding power; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Air release channels for fast, easy, bub.. |