3M Scotchcal™ IJ355%-10 Changeable Graphic Film

Category Polymer , Film
Manufacturer 3M
Trade Name ScotchCal™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotchcal™ IJ355%-10 Changeable Graphic Film.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
4-mil, opaque white vinyl film with a matte finish; Excellent hiding power; Pressure-sensitive adhesive; Changeable for clean removable without heat or chemicalsInformation provided by 3M
Physical Properties Metric English Comments
Thickness 102 microns
4.00 mil
without adhesive
114 - 127 microns
4.50 - 5.00 mil
with adhesive
Mechanical Properties Metric English Comments
Tensile Strength at Break 23.3 MPa
3380 psi
Peel Strength 0.105 kN/m
0.600 pli
Adhesion to Fruehauf pre-painted panels
0.316 kN/m
1.80 pli
Adhesion to Aluminum, anodized
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 38.0 °C
100 °F
Minimum Service Temperature, Air -2.00 °C
28.4 °F