Polymer Property : Peel Strength = 0.316 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Peel Strength 0.316 kN/m
1.80 pli
Adhesion to Aluminum, anodized
3M Controltac™ 8655C ES Changeable Graphic Film with Comply™ Adhesive
3M™ Controlact™ Plus Changeable Graphic Film with Comply™ Adhesive 8655C ES combines the features found in Controltac and Comply adhesive technologies, including pressure activation, positionabil..
Peel Strength 0.316 kN/m
1.80 pli
Adhesion to Aluminum, anodized
3M Scotchcal™ IJ355%-10 Changeable Graphic Film
4-mil, opaque white vinyl film with a matte finish; Excellent hiding power; Pressure-sensitive adhesive; Changeable for clean removable without heat or chemicalsInformation provided by 3M
Peel Strength 0.316 kN/m
1.80 pli
Adhesion to Fruehauf pre-painted panels
3M Controltac™ 160C Graphic Film with Comply™ Adhesive
4-mil, opaque white, opaque black and translucent white vinyl film with a matte finish; Pressure-activated adhesives for easy sliding, tacking, snap up and repositioning; Film series 160C-10 also ha..
Peel Strength 0.316 kN/m
1.80 pli
Adhesion to Aluminum, anodized
3M Controltac™ 3500C Changeable Graphic Film with Comply™ Adhesive
4-mil, opaque white vinyl film with a matte finish; Excellent hiding power; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Air release channels for fast, easy, bub..