Mechanical Properties Metric English Comments
Peel Strength 0.280 kN/m
1.60 pli
Neoprene Rubber, 180°, after 48 hrs at 23°C
3M Fastbond™ 4224-NF Pressure Sensitive Adhesives
3M™ Fastbond™ Pressure Sensitive Adhesive 4224-NF is a water-based, permanently pressure sensitive adhesive with excellent initial tack and good bond strength.Information provided by 3M
Peel Strength 0.280 kN/m
1.60 pli
Glass, 180°, after 48 hrs at 23°C
3M Fastbond™ 49 Insulation Adhesive
3M™ Fastbond™ Insulation Adhesive 49 is a water-based, high solids, fast tacking, pressure sensitive adhesive for bonding lightweight materials like fiberglass insulation, felt, shoddy, paper and ..