Mechanical Properties Metric English Comments
Seal Strength 610 g/25 mm

@Pressure 0.276 MPa,
Temperature 130 °C
610 g/in

@Pressure 40.0 psi,
Temperature 266 °F
Otto Bruger, 0.2 sec; ExxonMobil Method
ExxonMobil Bicor™ 35MB666 OPP Film
Product Description: A is a biaxially oriented transparent polypropylene film, acrylic coated tow sides. It provides outstanding performance on all packaging machines.Availability: Africa & Middle E..
Seal Strength 610 g/25 mm

@Pressure 0.276 MPa,
Temperature 130 °C
610 g/in

@Pressure 40.0 psi,
Temperature 266 °F
Otto Bruger, 0.2 sec; ExxonMobil Method
ExxonMobil Bicor™ 40MB666 OPP Film
Product Description: A is a biaxially oriented transparent polypropylene film acrylic coated two sides. It provides outstanding performance on all packaging machines.Availability: Africa & Middle Ea..
Seal Strength 610 g/25 mm

@Pressure 0.276 MPa,
Temperature 130 °C
610 g/in

@Pressure 40.0 psi,
Temperature 266 °F
Otto Brugger, 0.5 sec; ExxonMobil Method
ExxonMobil Oppalyte™ 42MH647 OPP Film
Product Description: A super white opaque, modified higher density, biaxially oriented polypropylene film, acrylic coated two sides. It provides outstanding performance on all packaging machines.Ava..
Seal Strength 610 g/25 mm

@Pressure 0.276 MPa,
Temperature 130 °C
610 g/in

@Pressure 40.0 psi,
Temperature 266 °F
Otto Brugger, 0.5 sec; ExxonMobil Method
ExxonMobil Oppalyte™ 52MH647 OPP Film
Product Description: A super white opaque, modified higher density, biaxially oriented polypropylene film, acrylic coated two sides. It provides outstanding performance on all packaging machines.Ava..