Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, TD | 570 MPa | 82700 psi | ASTM D882 |
Total PPH M3661 Metallocene Isostatic Polypropylene Polymer, Cast Film Extrusion TOTAL Petrochemicals Polypropylene M3661 is an isostatic form of homopolymer made via TOTAL proprietary metallocene catalyst technologyRecommended Applications. M3661 is a medium molecular weight m.. |