Polymer Property : 1% Secant Modulus, TD = 570 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
1% Secant Modulus, TD 570 MPa
82700 psi
ASTM D882
Total PPH M3661 Metallocene Isostatic Polypropylene Polymer, Cast Film Extrusion
TOTAL Petrochemicals Polypropylene M3661 is an isostatic form of homopolymer made via TOTAL proprietary metallocene catalyst technologyRecommended Applications. M3661 is a medium molecular weight m..