Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, TD | 53.1 MPa | 7700 psi | ASTM D882 |
ExxonMobil Escorene™ FL 00018 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: FL 00018 is a copolymer of ethylene and vinyl acetate. It offers combines toughness, good optical and sealing properties and low gel. In particular, its good behavior in high fr.. |
|||
1% Secant Modulus, TD | 53.1 MPa | 7700 psi | ASTM D882 |
ExxonMobil Escorene™ UL 00018 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: UL 00018 is a fractional MI copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: Yes Applic.. |