Category Polymer , Thermoplastic , Ethylene Vinyl Acetate
Manufacturer Exxon Chemical
Trade Name Escorene™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Escorene™ UL 00018 Ethylene Vinyl Acetate Copolymer (European Grade).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: UL 00018 is a fractional MI copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: Yes Applications:Agricultural FilmCompoundingProfile ExtrusionThick FilmWire and Cable Compounds Information provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.941 g/cc
0.0340 lb/in³
ExxonMobil method
Vinyl Acetate Content 17.5 %
17.5 %
ExxonMobil method
Melt Flow 0.37 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.37 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 550 %
550 %
ASTM D882
Film Elongation at Break, TD 650 %
650 %
ASTM D882
Film Tensile Strength at Break, MD 31.7 MPa
4600 psi
ASTM D882
Film Tensile Strength at Break, TD 31.7 MPa
4600 psi
ASTM D882
1% Secant Modulus, MD 51.0 MPa
7400 psi
ASTM D882
1% Secant Modulus, TD 53.1 MPa
7700 psi
ASTM D882
Thermal Properties Metric English Comments
Melting Point <= 187 °C
<= 369 °F
Peak Melting Point; ExxonMobil method
Vicat Softening Point 66.1 °C
151 °F
ASTM D1525
Copyright © lookpolymers.com All Rights Reserved