Polymer Property : 1% Secant Modulus, TD = 77.2 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
1% Secant Modulus, TD 77.2 MPa
11200 psi
ASTM D882
ExxonMobil ESCOR™ AT 310 Cast Film Resin  (discontinued **)
ESCOR AT 310 is an acid terpolymer which provides excellent adhesion to a variety of polar and non-polar materials such as metals, glass, polyolefins, polyamides, polyesters, etc. It is suitable fo..
1% Secant Modulus, TD 77.2 MPa
11200 psi
ASTM D882
ExxonMobil EXACT™ 3128 Plastomer for Blown Film Applications
Product Description: Exact 3128 is an ethylene-based butene plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. It is designed fro both monolayer and multilayer coextruded ..
1% Secant Modulus, TD 77.2 MPa
11200 psi
ASTM D882
ExxonMobil EXACT™ 3132 Plastomer for Blown Film Applications
Product Description: Exact 3132 is an ethylene-based hexene plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. Exact 3132 is designed for both monolayer and multilayer blo..