Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, TD | 77.2 MPa | 11200 psi | ASTM D882 |
ExxonMobil ESCOR™ AT 310 Cast Film Resin
(discontinued **) ESCOR AT 310 is an acid terpolymer which provides excellent adhesion to a variety of polar and non-polar materials such as metals, glass, polyolefins, polyamides, polyesters, etc. It is suitable fo.. |
|||
1% Secant Modulus, TD | 77.2 MPa | 11200 psi | ASTM D882 |
ExxonMobil EXACT™ 3128 Plastomer for Blown Film Applications Product Description: Exact 3128 is an ethylene-based butene plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. It is designed fro both monolayer and multilayer coextruded .. |
|||
1% Secant Modulus, TD | 77.2 MPa | 11200 psi | ASTM D882 |
ExxonMobil EXACT™ 3132 Plastomer for Blown Film Applications Product Description: Exact 3132 is an ethylene-based hexene plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. Exact 3132 is designed for both monolayer and multilayer blo.. |