Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, TD | 40.0 MPa | 5800 psi | ASTM D882 |
ExxonMobil Optema® TC-110 Blown Ethylene Methyl Acrylate Product Description: Optema TC 110 is an ethylene methyl acrylate copolymer specifically formulated to offer extrusion and property performance for blown film applications. It produces a soft, elast.. |