Polymer Property : 1% Secant Modulus, TD = 51.7 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
1% Secant Modulus, TD 51.7 MPa
7500 psi
ASTM D882
ExxonMobil Optema® TC-114 Blown Ethylene Methyl Acrylate
Product Description: Optema TC 114 is an ethylene methyl acrylate copolymer specifically formulated to offer extrusion and property performance for blown film applications. It produces a soft, elast..