Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, TD | 365 MPa | 53000 psi | ASTM D882 |
ExxonMobil Enable™ 27-03CH Metallocene Polyethylene Resin (European Grade) Product Description: Enable 27-03HH is a metallocene ethylene-hexene copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact and .. |