Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, TD | 227 MPa | 32900 psi | ASTM D-882 |
Bapolene® 122B Polyethylene, Film Grade Bapolene LL122B is a general purpose LLDPE for blown film extrusion. This resin offers excellent tensile and toughness properties. Contains no slip and no antiblock additives. This product meets .. |