Bapolene® 122B Polyethylene, Film Grade

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE
Manufacturer Bapolene®
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bapolene® 122B Polyethylene, Film Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Bapolene LL122B is a general purpose LLDPE for blown film extrusion. This resin offers excellent tensile and toughness properties. Contains no slip and no antiblock additives. This product meets FDA standards for food contact applications.Applications: Industrial bags, shipping sacks, frozen food packaging, trash bags. Film properties are based on a thickness of 1.0 mil, blow-up ratio of 2.5:1 and 0.1 mm/mm-min Initial Strain Rate.Bapolene® and Bapolan® are registered trademarks of Bamberger Polymers, Inc. Information provided by Bamberger Polymers
Physical Properties Metric English Comments
Density 0.918 g/cc
0.0332 lb/in³
ASTM D1505
Thickness 25.4 microns
1.00 mil
2.5:1 blow-up ratio
Melt Flow 1.0 g/10 min
1.0 g/10 min
ASTM D-1238
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 10.3 MPa
1490 psi
ASTM D-882
Film Tensile Strength at Yield, TD 10.5 MPa
1530 psi
ASTM D-882
Film Elongation at Break, MD 595 %
595 %
ASTM D-882
Film Elongation at Break, TD 795 %
795 %
ASTM D-882
Elmendorf Tear Strength MD 110 g
110 g
ASTM D-1922
Elmendorf Tear Strength TD 490 g
490 g
ASTM D-1922
Dart Drop Test 90.0 g
0.198 lb
ASTM D-1709A
Film Tensile Strength at Break, MD 38.7 MPa
5620 psi
ASTM D-882
Film Tensile Strength at Break, TD 28.3 MPa
4100 psi
ASTM D-882
1% Secant Modulus, MD 208 MPa
30200 psi
ASTM D-882
1% Secant Modulus, TD 227 MPa
32900 psi
ASTM D-882
Optical Properties Metric English Comments
Haze 18.5 %
18.5 %
ASTM D-1003
Gloss 35 %
35 %
ASTM D-2457
Descriptive Properties Value Comments
Process Film
Region Europe/Turkey
Bamberger Polymers Distribution
International
Bamberger Polymers Distribution
Mexico
Bamberger Polymers Distribution
US & Canada
Bamberger Polymers Distribution