Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, TD | 276 MPa | 40000 psi | ASTM D882 |
LyondellBasell Petrothene® NA324009 Low Density Polyethylene (Film Grade) ApplicationsPETROTHENE NA 324 is a series of homopolymer resins specifically designed for overwrap packaging. NA 324 provides excellent optical properties and good stiffness for improved machineabi.. |
|||
1% Secant Modulus, TD | 276 MPa | 40000 psi | ASTM D882 |
Westlake EB169 Low Density Polyethylene Westlake EB169 is a low-density polyethylene with high stiffness designed for beverage shrink overwrap and towel/tissue packaging. It has good toughness and blends well with LLDPE resins.Application.. |
|||
1% Secant Modulus, TD | 276 MPa | 40000 psi | ASTM D882 |
Westlake EF1807 Low Density Polyethylene Westlake Polyethylene EF1807 is a low density formulation suggested for film applications that require toughness.Application/UsesShrink filmFrozen food packagingFDA: This material complies with FDA .. |
|||
1% Secant Modulus, TD | 276 MPa | 40000 psi | ASTM D882 |
Westlake EN1807AA Low Density Polyethylene WESTLAKE polyethylene EN1807 is a fractional-melt low- density formulation suggested for film applications requiring high impact strength, high tear strength, and very good optical properties, such .. |
|||
1% Secant Modulus, TD | 276 MPa | 40000 psi | ASTM D882 |
Westlake Hifor Clear SC74558 Linear Low Density Polyethylene WESTLAKE Hifor Clear Polyethylene SC74558 is a high strength and high clarity linear low density polyethylene designed for blown film extrusion that contains medium slip and low antiblock additives... |
|||
1% Secant Modulus, TD | 276 MPa | 40000 psi | ASTM D882 |
Westlake Hifor SC74557 Linear Low Density Polyethylene WESTLAKE Hifor Clear Polyethylene SC74557 is a high strength and high clarity linear low density polyethylene designed for blown film extrusion that contains no slip and low antiblock. Films produc.. |