Material Notes:
Westlake EB169 is a low-density polyethylene with high stiffness designed for beverage shrink overwrap and towel/tissue packaging. It has good toughness and blends well with LLDPE resins.Application/UsesBeverage overwrap shrink filmLight and medium duty produce bagsClarity packagingFDA: This material complies with FDA regulations in 21 CFR, section 177.1520. Kosher Compliant.All information provided by Westlake Chemical
Physical Properties Metric English Comments
Density 0.927 g/cc
0.0335 lb/in³
ASTM D1505
Thickness 31.8 microns
1.25 mil
Melt Flow 1.6 g/10 min
1.6 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 300 %
300 %
ASTM D882
Film Elongation at Break, TD 800 %
800 %
ASTM D882
Dart Drop 3.35 g/micron
85.0 g/mil
ASTM D1709
Film Tensile Strength at Break, MD 19.3 MPa
2800 psi
ASTM D882
Film Tensile Strength at Break, TD 17.9 MPa
2600 psi
ASTM D882
1% Secant Modulus, MD 234 MPa
34000 psi
ASTM D882
1% Secant Modulus, TD 276 MPa
40000 psi
ASTM D882
Optical Properties Metric English Comments
Haze 6.5 %
6.5 %
ASTM D1003
Gloss 65 %
65 %
at 45º; ASTM D2457
Processing Properties Metric English Comments
Melt Temperature 182 - 199 °C
360 - 390 °F
with BUR of 1.5:1 or higher
Blow-up Ratio (BUR) 2.5
2.5
Descriptive Properties Value Comments
Process Film