Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, TD | 260 MPa | 37700 psi | ASTM D882 |
SABIC 218 Series Linear Low Density Polyethylene for Blown Film Product Description: 218 series resins are Linear Low Density Polyethylene grades suitable for general purpose packaging. They are easy to process giving good tensile properties, impact strength a.. |
|||
1% Secant Modulus, TD | 260 MPa | 37700 psi | 3 mil; ASTM D882 |
NOVA Chemicals Sclair® FP026-F Octene LLDPE Film Resin Features: Moderate toughness and strengthGood stiffnessEasy processabilityExcellent seal properties Applications: Heavy duty shipping sacks requiring moderate toughness and high stiffnessIndustrial .. |