Mechanical Properties Metric English Comments
1% Secant Modulus, TD 155 MPa
22500 psi
ISO 527-3
Polimeri Europa Clearflex® H&T CMH 108 Octene Copolymer Linear Low Density Polyethylene
Clearflex H&T CMH 108 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidants, suitable for cast film extrusion. Stretch films obtained from Clearflex H&T CMH 108 show e..