Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, TD | 155 MPa | 22500 psi | ISO 527-3 |
Polimeri Europa Clearflex® H&T CMH 108 Octene Copolymer Linear Low Density Polyethylene Clearflex H&T CMH 108 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidants, suitable for cast film extrusion. Stretch films obtained from Clearflex H&T CMH 108 show e.. |