Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, TD | 155.0 MPa | 22480 psi | ASTM D882 |
NOVA Chemicals Surpass® HPs900-C Octene sLLDPE Film Resin Features: Easy processabilityExceptional clarity and glossLow gelExcellent seal properties Applications: High clarity applications Lamination film Coextruded sealant layerHigh toughness filmInformat.. |