Polymer Property : 1% Secant Modulus, TD = 193600 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
1% Secant Modulus, TD 1335 MPa
193600 psi
ASTM D 882
NOVA Chemicals Surpass® HPs167-AB Homopolymer sHDPE Film Resin
HPs167-AB complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food.NOVA Che..