Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, TD | 188 MPa | 27300 psi | ASTM D 882 |
NOVA Chemicals Surpass® FPs021-F Octene sLLDPE Film Resin, 25 Micron Film FPs021-F complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food.NOVA Chem.. |
|||
1% Secant Modulus, TD | 188 MPa | 27200 psi | ASTM D882 |
ExxonMobil LD 313.NF Blown Film Resin LD 313.NF is a 3 wt% vinyl acetate copolymer. The vinyl acetate content of this resin provides good heat sealing and good cold temperature toughness when compared to LDPE homopolymers.Information pr.. |