Mechanical Properties Metric English Comments
1% Secant Modulus, TD 1070 MPa
155000 psi
ASTM D822
LyondellBasell Alathon® M6020 High Density Polyethylene
ApplicationsALATHON 6020 is a medium molecular high density weight homopolymer for use in blown or cast film applications. This resin provides extremely low gel content and high stiffness. Typica..
1% Secant Modulus, TD 1070 MPa
155000 psi
ASTM D882
Chevron Phillips MarFlex® 9656 HDPE Blown Film Resin
Resin Type: high density, linear polyethylene.Characteristics: copolymerization enhances film toughness, good drawdown, density level gives good machinability, blend well with LLDPEApplications: not..