LyondellBasell Alathon® M6020 High Density Polyethylene

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Film Grade
Manufacturer LyondellBasell (former Equistar)
Trade Name Alathon®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Alathon® M6020 High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ApplicationsALATHON 6020 is a medium molecular high density weight homopolymer for use in blown or cast film applications. This resin provides extremely low gel content and high stiffness. Typical applications include dry food packaging, overwrap, and WVTRRegulatory StatusM 6020 meets the requirements of Food and Drug Administration regulation, 21 CFR 177.1520. This regulation allows the use of this olefin polymer in "…articles or components of articles intended for use in contact with food." Specific limitations or conditions of use may apply. Contact your Equistar sales representative for more information. Processing TechniquesSpecific recommendations for processing M 6020 can only be made when the processing conditions, equipment and end use are known. For further suggestions, please contact your Equistar sales representative.Typical Extrusion Conditions2.0 Mil Film; Melt Temperature- 390-410°F(199-210°C)This product is from the former Equistar product line.
Physical Properties Metric English Comments
Density 0.960 g/cc
0.0347 lb/in³
ASTM D792
Thickness 50.8 microns
2.00 mil
Melt Flow 2.0 g/10 min
2.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 22.8 MPa
3300 psi
ASTM D822
Film Tensile Strength at Yield, TD 21.4 MPa
3100 psi
ASTM D822
Film Elongation at Break, MD 860 %
860 %
ASTM D822
Film Elongation at Break, TD 850 %
850 %
ASTM D822
Elmendorf Tear Strength MD 22 g
22 g
ASTM D1922
Elmendorf Tear Strength TD 500 g
500 g
ASTM D1922
1% Secant Modulus, MD 827 MPa
120000 psi
ASTM D822
1% Secant Modulus, TD 1070 MPa
155000 psi
ASTM D822
Processing Properties Metric English Comments
Melt Temperature 199 - 210 °C
390 - 410 °F
Typical Extrusion
Users viewing this material also viewed the following: