Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, TD | 82.7 MPa | 12000 psi | ASTM D882 |
ExxonMobil Escorene™ UL 00014 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: UL 00014 is a fractional MI copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: Yes Applic.. |
|||
1% Secant Modulus, TD | 82.7 MPa | 12000 psi | ASTM D882 |
ExxonMobil Escorene™ LD 708.62 Ethylene Vinyl Acetate Copolymer Product Description: Escorene Ultra UL 708.62 is a 14.9% VA copolymer film resin. Film made from LD 708.62 exhibits good impact strength and superior heat sealabilty.Availability: Latin America, Nor.. |