Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, MD | 427 MPa | 62000 psi | ASTM D882 |
ExxonMobil Enable™ 35-05HH Metallocene Polyethylene Resin Product Description: Enable 35-05HH is a metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact and .. |
|||
1% Secant Modulus, MD | 427 MPa | 62000 psi | ASTM D882 |
ExxonMobil Enable™ 35-05HH Metallocene Polyethylene Resin (European Grade) Product Description: Enable 35-05HH is a metallocene ethylene-hexene copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact and .. |