Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, MD | 221 MPa | 32000 psi | ASTM D638 |
LyondellBasell Petrothene® GA502022 Linear Low Density Polyethylene ApplicationsThe PETROTHENE GA 502 series of resins are pelletized linear low density polyethylene for film extrusion applications requiring excellent drawdown and toughness. These pelletized produc.. |
|||
1% Secant Modulus, MD | 221 MPa | 32000 psi | ASTM D638 |
LyondellBasell Petrothene® GA502024 Linear Low Density Polyethylene ApplicationsThe PETROTHENE GA 502 series of resins are pelletized linear low density polyethylene for film extrusion applications requiring excellent drawdown and toughness. These pelletized produc.. |
|||
1% Secant Modulus, MD | 221 MPa | 32000 psi | ASTM D638 |
LyondellBasell Petrothene® GA502023 Linear Low Density Polyethylene ApplicationsThe PETROTHENE GA 502 series of resins are pelletized linear low density polyethylene for film extrusion applications requiring excellent drawdown and toughness. These pelletized produc.. |
|||
1% Secant Modulus, MD | 221 MPa | 32000 psi | ASTM D882 |
Westlake EF1807 Low Density Polyethylene Westlake Polyethylene EF1807 is a low density formulation suggested for film applications that require toughness.Application/UsesShrink filmFrozen food packagingFDA: This material complies with FDA .. |
|||
1% Secant Modulus, MD | 221 MPa | 32000 psi | ASTM D882 |
Westlake EN1807AA Low Density Polyethylene WESTLAKE polyethylene EN1807 is a fractional-melt low- density formulation suggested for film applications requiring high impact strength, high tear strength, and very good optical properties, such .. |
|||
1% Secant Modulus, MD | 221 MPa | 32000 psi | ASTM D882 |
Westlake Hifor LT74104 Linear Low Density Polyethylene WESTLAKE Hifor Polyethylene LT74104 is a high strength linear low density polyethylene containing no slip or antiblock. It is designed for blown film applications and is well suited for consumer an.. |
|||
1% Secant Modulus, MD | 221 MPa | 32000 psi | ASTM D882 |
Westlake Hifor LT74105 Linear Low Density Polyethylene WESTLAKE Hifor Polyethylene LT74105 is a high strength linear low density polyethylene containing medium slip and medium antiblock. It is designed for blown film applications and is well suited for.. |
|||
1% Secant Modulus, MD | 221 MPa | 32000 psi | ASTM D882 |
Westlake Hifor LT74113 Hexene Linear Low Density Polyethylene WESTLAKE Hifor Polyethylene LT74113 is a high strength hexene linear low density polyethylene containing no slip and medium antiblock. It is designed for blown film applications and is well suited .. |
|||
1% Secant Modulus, MD | 221 MPa | 32000 psi | ASTM D882 |
Westlake Hifor LT74119 Linear Low Density Polyethylene WESTLAKE HIFOR Polyethylene LT74119 is a high strength linear low density polyethylene containing medium slip and high antiblock and it contains processing aid. It is designed for blown film applic.. |
|||
1% Secant Modulus, MD | 221 MPa | 32000 psi | ASTM D882 |
Westlake Hifor LT74147 Linear Low Density Polyethylene WESTLAKE HIFOR Polyethylene LT74147 is a high strength linear low density polyethylene containing medium slip and high antiblock. It is designed for blown film applications and is well suited for c.. |
|||
1% Secant Modulus, MD | 221 MPa | 32000 psi | ASTM D882 |
ExxonMobil LDPE LD 123.LN Low Density Polyethylene Resin Product Description: LD 123.LN blown film grade offers an excellent balance of optical and strength properties for general purpose clear film applications.Availability: Latin America, North America .. |
|||
1% Secant Modulus, MD | 221 MPa | 32000 psi | ASTM D882 |
ExxonMobil LDPE LD 150AC Low Density Polyethylene Resin Product Description: LD 150 series are LDPE grades, offering good blend mechanical properties and stiffness. Several additive packages are available according to the required surface properties.Avai.. |
|||
1% Secant Modulus, MD | 221 MPa | 32000 psi | ASTM D882 |
ExxonMobil LDPE LD 150BW Low Density Polyethylene Resin Product Description: LD 150 series are LDPE grades, offering good blend mechanical properties and stiffness. Several additive packages are available according to the required surface properties.Avai.. |
|||
1% Secant Modulus, MD | 221 MPa | 32000 psi | ASTM D882 |
ExxonMobil LDPE LD 159AC Low Density Polyethylene Resin Product Description: LD 159AC is an LDPE grade, which offers good draw down combined with good mechanical strength. Availability: Africa & Middle East and Europe Additive: Antiblock: 450 ppmSlip: 5.. |
|||
1% Secant Modulus, MD | 221 MPa | 32000 psi | ASTM D882 |
ExxonMobil LDPE LD 165BW1 Low Density Polyethylene Resin Product Description: LD 165BW1 is a fractional melt index LDPE, with medium optical properties.Availability: Latin America, North America and South America Applications: Agricultural FilmBlend Part.. |