Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, MD | 192 MPa | 27800 psi | ASTM D882 |
ExxonMobil LD 135.09 Blown Film Resin
(discontinued **) LD 135.09 is a homopolymer film resin with good clarity. Applications include food packaging, light to medium duty bags, and textile packaging.Information provided by ExxonMobil Chemical |