Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, MD | 179 MPa | 25900 psi | ASTM D882 |
Chevron Phillips Dynex™ D605A6 Enhanced LLDPE Blown Film Resin
(discontinued **) Resin Type: enhanced linear low density polyethylene, high antiblock, and processing aid additiveCharacteristics: superior dart impact, optical, hot-tack and heat seal properties, good drawdown, can.. |