Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, MD | 179 MPa | 25900 psi | ASTM D882 |
Chevron Phillips Dynex™ D605A6 Enhanced LLDPE Blown Film Resin
(discontinued **) Resin Type: enhanced linear low density polyethylene, high antiblock, and processing aid additiveCharacteristics: superior dart impact, optical, hot-tack and heat seal properties, good drawdown, can.. |
|||
1% Secant Modulus, MD | 179 MPa | 26000 psi | ASTM D882 |
ExxonMobil Exceed™ 1518EC Tough Premium Film Resin
(discontinued **) Exceed 1518EC resin is a hexene copolymer produced using ExxonMobil Chemicals EXXPOL® Technology. Films made from 1518EC resin have outstanding tensile, impact strength and puncture. These superi.. |
|||
1% Secant Modulus, MD | 179 MPa | 26000 psi | ASTM D882 |
LyondellBasell Petrothene® NA345009 Low Density Polyethylene (Film Extrusion) ApplicationsPETROTHENE NA 345 is a series of homopolymer resins combining premium clarity with strength and stiffness. In addition, NA 345 exhibits good impact strength on both flat and creased fil.. |
|||
1% Secant Modulus, MD | 179 MPa | 26000 psi | ASTM D882 |
LyondellBasell Petrothene® NA345013 Low Density Polyethylene (Film Extrusion) ApplicationsPETROTHENE NA 345 is a series of homopolymer resins combining premium clarity with strength and stiffness. In addition, NA 345 exhibits good impact strength on both flat and creased fil.. |
|||
1% Secant Modulus, MD | 179 MPa | 26000 psi | ASTM D882 |
LyondellBasell Petrothene® NA345184 Low Density Polyethylene (Film Extrusion) ApplicationsPETROTHENE NA 345 is a series of homopolymer resins combining premium clarity with strength and stiffness. In addition, NA 345 exhibits good impact strength on both flat and creased fil.. |
|||
1% Secant Modulus, MD | 179 MPa | 26000 psi | ASTM D882 |
LyondellBasell Petrothene® NA345196 Low Density Polyethylene (Film Extrusion) ApplicationsPETROTHENE NA 345 is a series of homopolymer resins combining premium clarity with strength and stiffness. In addition, NA 345 exhibits good impact strength on both flat and creased fil.. |
|||
1% Secant Modulus, MD | 179 MPa | 26000 psi | ASTM D882 |
LyondellBasell Petrothene® NA963083 Low Density Polyethylene ApplicationsPETROTHENE NA 963 is a series of resins formulated with special antiblock additive and designed for a wide variety of industrial film applications where high impact strength and excellen.. |
|||
1% Secant Modulus, MD | 179 MPa | 26000 psi | ASTM D882 |
LyondellBasell Petrothene® NA967000 Low Density Polyethylene, Film Extrusion Grade Petrothene NA967000 is a low density polyethylene resin designed for blown film, general purpose and industrial packaging applications. NA967000 exhibits good processing characteristics and impact s.. |
|||
1% Secant Modulus, MD | 179 MPa | 26000 psi | ASTM D882 |
Westlake EF403 Low Density Polyethylene WESTLAKE polyethylene EF403 is a fractional melt low-density formulation suggested for use in clarity shrink applications. This LDPE formula exhibits excellent skrinkability, and has very good optic.. |
|||
1% Secant Modulus, MD | 179 MPa | 26000 psi | ASTM D882 |
Westlake EF403 Low Density Polyethylene WESTLAKE polyethylene EB403 is a fractional melt low-density formulation suggested for use in clarity shrink applications. This LDPE formula exhibits excellent shrinkability, and has very good optic.. |
|||
1% Secant Modulus, MD | 179 MPa @Thickness 0.0254 mm |
26000 psi @Thickness 0.00100 in |
ASTM D882A |
Total L425 HDPE Film Blown film polyethylene grade. Provides excellent bubble stability, exceptional tear strength, high impact and puncture resistance, outstanding clarity and gloss, good stiffness, excellent compatibi.. |
|||
1% Secant Modulus, MD | 179 MPa | 26000 psi | Cast Film at 1 mil; ASTM D-882 |
Chevron Phillips MarFlex® 7114 Polyethylene; LLDPE Hexene linear low density polyethylene. This LLDPE is tailored for applications that require: Good stiffness at thin gaugesGood drawdownExcellent processabilityCan use straight or in blends with L.. |
|||
1% Secant Modulus, MD | 179 MPa | 26000 psi | ASTM D882 |
ExxonMobil Exceed™ 1518HA Metallocene Polyethylene Resin Product Description: Exceed 1518HA is a metallocene ethylene-hexene copolymer. Films made from Exceed 1518HA have outstanding tensile, impact strength and puncture. These superior strength propertie.. |
|||
1% Secant Modulus, MD | 179 MPa | 26000 psi | ASTM D882 |
ExxonMobil Exceed™ 2018KB Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 2018KB is a metallocene catalyzed ethylene-hexene copolymer. Films made from Exceed 2018KB have outstanding tensile, impact strength, and puncture. These superior strengt.. |
|||
1% Secant Modulus, MD | 179 MPa | 26000 psi | ASTM D882 |
ExxonMobil LD 102.LC Thin Gauged Film Resin L Product Description: LD 102.LC is a formulated homopolymer, garment film resin with good toughness. It is capable of being drawndown to thing gauges.Availability: Latin America, North America and .. |
|||
1% Secant Modulus, MD | 179 MPa | 26000 psi | ASTM D882 |
ExxonMobil LDPE LD 102.LC Low Density Polyethylene Resin Product Description: LD 102.LC is a formulated homopolymer, garment film resin with good toughness. It is capable of being drawn down to thing gauges.Availability: Latin America, North America and S.. |
|||
1% Secant Modulus, MD | 179 MPa | 26000 psi | ASTM D882 |
ExxonMobil LDPE LD 160AT Low Density Polyethylene Resin Product Description: LD 160 series are LDPE grades, which offer good draw down and optical properties.Availability: Africa & Middle East, Asia Pacific, Latin America, North America and South America.. |
|||
1% Secant Modulus, MD | 179 MPa | 26000 psi | ASTM D882 |
ExxonMobil LLDPE LL 1002.09 Linear Low Density Polyethylene Resin Product Description: LL 1002 resins are butane LLDPE designed for the blown film process. Films made form LL 1002 resins have very good tensile and toughness properties. LL 1002.09 is a granular mat.. |
|||
1% Secant Modulus, MD | 179 MPa | 26000 psi | ASTM D882 |
ExxonMobil LLDPE LL 1002.80 Linear Low Density Polyethylene Resin Product Description: LL 1002 resins are butane LLDPE designed for the blown film process. Films made form LL 1002 resins have very good tensile and toughness properties. LL 1002.09 is a granular mat.. |
|||
1% Secant Modulus, MD | 179 MPa | 26000 psi | ASTM D882 |
ExxonMobil LLDPE LL 1002X75 Linear Low Density Polyethylene Resin Product Description: LL 1002 resins are butane LLDPE designed for the blown film process. Films made form LL 1002 resins have very good tensile and toughness properties. LL 1002.09 is a granular mat.. |
|||
1% Secant Modulus, MD | 179 MPa | 26000 psi | ASTM D882 |
ExxonMobil Exceed™ 1018EB Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 1018EB is a metallocene ethylene-hexene copolymers. Films are made of Exceed 1018EB have outstanding tensile, impact, puncture resistance and low temperature properties. .. |
|||
1% Secant Modulus, MD | 179 MPa @Thickness 0.0317 mm |
26000 psi @Thickness 0.00125 in |
ASTM D-882 |
Bapolene® 108A Low Density Polyethylene Film Extrusion Resin Bapolene® 108A is an LDPE for blown film. It contains 2500 ppm antiblock additive. This product meets the Food and Drug Administration requirements of 21CFR177.1520.Applications: General purpose p.. |
|||
1% Secant Modulus, MD | 179 MPa @Thickness 0.0356 mm |
26000 psi @Thickness 0.00140 in |
ASTM D-882 |
Bapolene® 270F Low Density Polyethylene Film Extrusion Resin Bapolene® 270F is an LDPE for blown film requiring superior clarity. It contains 1600 ppm antiblock and 725 ppm slip additives. This product meets the Food and Drug Administration requirements of .. |
|||
1% Secant Modulus, MD | 179 MPa | 26000 psi | ASTM D882 |
ExxonMobil Exceed™ 3527PA Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 3527PA is a metallocene ethylene-hexene copolymer. Films made of Exceed 3527PA have high modulus and outstanding tensile, impact and puncture resistance properties. These.. |