Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, MD | 170 MPa | 24700 psi | ISO 527-3 |
Polimeri Europa Clearflex® H&T FGH 196 Hexene Copolymer Linear Low Density Polyethylene Clearflex H&T FGH 196 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidants and processing aid, suitable for blown film extrusion.Films obtained from Clearflex H&T FGH .. |
|||
1% Secant Modulus, MD | 170 MPa | 24700 psi | ISO 527-3 |
Polimeri Europa Riblene® FC 20 Low Density Polyethylene - Blown Film Extrusion Riblene FC 20 is a high molecular weight low density polyethylene resin (LDPE) suitable for blown film extrusion. Riblene FC 20 is characterized by a high melt strength leading to a good bubble sta.. |
|||
1% Secant Modulus, MD | 170 MPa | 24700 psi | ISO 527-3 |
Polimeri Europa Riblene® FL 24 Low Density Polyethylene - Blown Film Extrusion Riblene FL 24 is a low density polyethylene (LDPE) with added slip and antiblocking agents, suitable for blown film extrusion. Riblene FL 24 is characterized by a good balance between processabilit.. |
|||
1% Secant Modulus, MD | 170 MPa | 24700 psi | ASTM D 882 |
NOVA Chemicals Novapol® PF-0218-B Butene Copolymer LLDPE Film Resin PF-0218-B complies with the U.S. FDA specifications for olefin polymers and may be used in the U.S. as an article or component of an article intended for use in contact with food, without temperatur.. |
|||
1% Secant Modulus, MD | 170 MPa | 24700 psi | ASTM D 882 |
NOVA Chemicals Novapol® PF-0218-E Butene Copolymer LLDPE Film Resin PF-0218-E complies with the U.S. FDA specifications for olefin polymers and may be used in the U.S. as an article or component of an article intended for use in contact with food, without temperatur.. |
|||
1% Secant Modulus, MD | 170 MPa | 24700 psi | ASTM-D882 |
Braskem FC31D LLDPE Blown Film Extrusion Polyethylene Copolymer The FC31D resin is a linear low-density polyethylene, copolymer of butene -1, produced by the solution process for blow film extrusion. It has excellent mechanical properties, especially hot tack. I.. |
|||
1% Secant Modulus, MD | 170 MPa | 24700 psi | ASTM-D882 |
Braskem LBH0120PBS LLDPE Blown Film Extrusion Polyethylene Copolymer LBH0120BPS is a LLDPE Hexene copolymer produced by Braskem. It is a general purpose product that shows a good processing performance balanced with good optical and mechanical properties as well as s.. |
|||
1% Secant Modulus, MD | 170 MPa | 24700 psi | ASTM D882 |
Braskem LH0820/30AF Blown Film Extrusion Linear Low Density Polyethylene Description: LH0820/30AF is a LLDPE hexene copolymer produced by Braskem. It offers outstanding processability combined with excellent mechanical properties. Very low gel amount.Applications: Lamina.. |
|||
1% Secant Modulus, MD | 170 MPa | 24700 psi | ASTM D882 |
Braskem Green PE SLH0820/30AF Blow Film Extrusion and Cast Film Extrusion Linear Low Density Polyethylene Description: SLH0820/30AF is a LLDPE hexene copolymer produced by Braskem. It offers outstanding processability combined with excellent mechanical properties. Very low gel amount. The minimum biobas.. |
|||
1% Secant Modulus, MD | 170 MPa | 24700 psi | ASTM-D882 |
Braskem LF218/21 LLDPE Cast and Blown Film Extrusion Polyethylene Copolymer LF218/21 is a LLDPE Butene copolymer produced by Braskem. It was specially designed to provide outstanding processing performance. Films obtained with this grade show good physical and optical prope.. |