Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, MD | 166 MPa | 24100 psi | ASTM D882 |
ExxonMobil LL 1235x70 Cast Film Resin
(discontinued **) LL 1235x70 is a butene LLDPE with improved stiffness. It can be used alone or as a component in packaging and industrial film.Information provided by ExxonMobil Chemical |