Polymer Property : 1% Secant Modulus, MD = 22800 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
1% Secant Modulus, MD 157 MPa
22800 psi
ASTM D882
ExxonMobil LD 102.74 Thin Gauged Film Resin  (discontinued **)
LD 102 series are homopolymer, good clarity, laundry and dry cleaning film resins capable of providing a tough film in very thin gaugesInformation provided by ExxonMobil Chemical