Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Yield Strength = 9800 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 67.6 MPa
9800 psi
ASTM D790
Spartech Korad® SP-9071 FR/ABS Flame Retardant Sheet
Description: Flame Retardant SheetKorad is a registered trademark of Polymer Extruded Products, Inc..Information provided by Spartech.
Flexural Yield Strength 67.6 MPa
9800 psi
ASTM D790
Spartech SP-9013 FR/ABS Flame Retardant Sheet
Description: Flame Retardant SheetInformation provided by Spartech.
Flexural Yield Strength 67.6 MPa
9800 psi
ASTM D790
Techmer ES Plastiblend® ABS FR IM
Availability: North AmericaForms: PelletsFeatures: Flame Retardant and High Impact ResistanceProcessing Method: Injection MoldingInformation provided by TP Composites, Inc.
Flexural Yield Strength 67.6 - 360 MPa
9800 - 52200 psi
Average value: 219 MPa Grade Count:155
Overview of materials for Polyetheretherketone, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Glass Fiber Filled". Each property range of values reported is minimum and maximum..