Polymer Property : Flexural Yield Strength = 83.91 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 83.91 MPa
12170 psi
Abatron AboCast 50-6/AboCure 50-1 Epoxy
Data provided by the manufacturer, Abatron, Inc. Motor oil viscosity, light amber color. Peak exothermic temperature is 160°C (320°F). Shelf life is 12+ months.