Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 80.0 - 80.0 MPa @Temperature 90.0 - 90.0 °C |
11600 - 11600 psi @Temperature 194 - 194 °F |
Average value: 80.0 MPa Grade Count:1 |
Overview of materials for Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled". Specific grades with glass content between 15.. |
|||
Flexural Yield Strength | 48.3 - 80.0 MPa | 7000 - 11600 psi | Average value: 65.6 MPa Grade Count:7 |
Overview of materials for Polypropylene with Glass Fiber + Bead Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Glass Fiber + Bead Filler". Each property range of values reported is minimum and max.. |
|||
Flexural Yield Strength | 70.0 - 80.0 MPa | 10200 - 11600 psi | ASTM D790 |
Chang Chun Plastic PBT2000 Fire Retardant PBT Information provided by Dowell Trading Company Ltd. |